Abstract: With the age increase of steel gate, defects such as rust, wear, cavitation, crack, deformation, loosen connecting rod, seizure of movable joint would occur. In review of the strength on the corroded and weakened cross section, to modify the allowable stress of structure material, reduction by age is not recommended.